16MnDR is pronounced as 16Mn low capacity, 16Mn means that the carbon content in the steel plate is about 0}.16%, D means low temperature and R means pressure vessel. Usually a high content of a chemical element in the steel needs to be marked in the material, such as 1.6% manganese is written as 16Mn, is used for -40 degree pressure vessels. Steel plate strength, plasticity, low-temperature toughness, aging impact indicators are more desirable, of which the strength, low-temperature impact indicators and have a large margin with steel plate.
16MnDR steel plate process: iron → converter → LF furnace → (VD) → continuous casting → stack cooling → slab inspection → heating → high-pressure water descaling → roughing → finishing → ACC cooling → hot straightening → finishing → flaw detection → normalisasi % e2�� Steel plate Sampling, inspection → Storage.
Delivery state of 16MnDR steel plate: the default is normalized delivery state, different delivery states need to be specified in the contract, can also do one, two, three levels of flaw detection, can also do Z15, Z25, Z35 and other Z to performance.
Suhu rendah keluli dengan baik keliatan dan kebolehkimpalan, has been widely used in a variety of liquid alkanes with storage containers and transmission pipelines, natural gas liquefaction plant, large liquefied natural gas, liquefied petroleum gas equipment and storage and transportation facilities, tankers for the delivery of liquefied natural gas, hydrogenation plants and other parts; for the production of reactors, heat Exchangers, Separators, Tanks, Ball tanks, tanks, Liquefied petroleum Gas tanks, Nuclear Power Reactors, pressure shells, boiler steamer package, liquefied Petroleum gas cylinders, high-pressure water pipes of hydropower stations, hydraulic turbine worm shells and other equipment and components.