EN10028-6 P690QHadalah keluli bijirin yang boleh dikimpal, baik - yang dipadamkan dan dipadamkan untuk kekuatan tinggi, digunakan untuk peralatan tekanan. "P690" menunjukkan kekuatan hasil minimum 690MPa,dan "QH" menandakan penamaan "kualiti", yang memerlukan tenaga impak minimum $ 27 $ j pada suhu−20∘𝐶
EN10028-6 P690QH Tekanan Kapal dan Komposisi Kimia Plat Keluli Dandang dan Harta Mekanikal
| Gred | C% | Si% | Mn% | P% | S% | N% | B% | CR% | Mo% | Cu% | Nb% | Ni% | Ti% | V% | Zr% |
| P690QH | 0.2 | 0.8 | 1.7 | 0.025 | 0.015 | 0. 015 | 0.005 | 1.5 | 0.7 | 0.3 | 0.06 | 2.5 | 0.05 | 0.12 | 0.15 |
| Gred keluli | Kekuatan hasil, untuk produk dalam mm, MPA | Kekuatan tegangan, MPA | Pemanjangan, %, min | ||||
| P690QH | t kurang daripada atau sama dengan 50 | 50<> | 100<> | t kurang daripada atau sama dengan 100 | 100<> | 14 | |
| 690 | 670 | 630 | 770-940 | 720-900 | |||
EN10028-6 P690QH Kapal Tekanan dan Aplikasi Plat Keluli Boiler
Kapal tindak balas kimia
EN10028-6 P690QH Dandang dan plat keluli tekanan digunakan dalam tindak balas sintesis (seperti menara sintesis ammonia dalam tumbuhan baja dan reaktor pempolimeran dalam tumbuhan kimia). Ia perlu menahan suhu dan tekanan yang tinggi (contohnya, menara sintesis ammonia beroperasi pada tekanan 30MPa dan suhu 450 darjah) dan kakisan sederhana (seperti gas hidrogen dan asid) untuk memastikan tiada kebocoran atau kegagalan struktur berlaku semasa proses tindak balas.
Tangki dan Menara Penyimpanan Petrokimia
EN10028 - 6 P690QH Tekanan suhu rendah Plat keluli digunakan dalam tangki penyimpanan untuk minyak mentah, gas asli cecair (LNG), dan gas petroleum cecair (LPG) Low - tangki simpanan suhu (seperti tangki simpanan LNG, dengan suhu serendah - 162 darjah) memerlukan plat keluli dengan ketangguhan suhu rendah yang sangat baik untuk mengelakkan patah rapuh keluli pada suhu rendah; Menara hidrogenasi tekanan tinggi (proses hidrofin petrokimia).
Kapal pertukaran haba
EN10028 - 6 P690QH Tinggi - Plat keluli dandang berkualiti digunakan dalam peralatan untuk pertukaran haba sederhana (seperti shell - dan penukar haba tiub dan penukar haba plat). Kerang dan helaian tiub mereka perlu menahan kejutan panas dan sejuk, memastikan rintangan keletihan, dan elakkan keretakan kimpalan yang disebabkan oleh perubahan suhu yang kerap.
Industri Metalurgi
"Kompor letupan panas relau" dalam tumbuhan keluli (yang menyimpan tinggi - udara panas suhu, dengan tekanan 0.5 - 1.5MPa dan suhu 1200 darjah) menggunakan suhu tinggi - "Autoclave" dalam peleburan logam yang tidak ferus (seperti autoklave larutan dalam peleburan tembaga hidrometallurgikal) perlu tahan kakisan asid, dan plat keluli tekanan EN10028-6 P690QH biasanya digunakan.
EN10028-6 P690QH Tekanan Kapal dan Plat Keluli Boiler Nama Lain
EN10028-6 P690QH Plat keluli dandang|EN10028-6 P690QH Tekanan Kapal Kapal Plate|EN10028-6 P690QH Penyimpanan Tangki Plat Keluli |
Keadaan tambahan
UT (pemeriksaan ultrasonik), AR (seperti yang dilancarkan panas sahaja), TMCP (pemprosesan kawalan mekanikal termal), N (dinormalisasi), q+t (dipadamkan dan marah), z arah arah (z15, z25, z35), charpy v -
Klik untuk mendapatkan contoh percuma
Sekiranya anda ingin mengetahui lebih lanjut mengenai produk GNEE, anda boleh menghantar e -mel kealloy@gneesteelgroup.com. Kami lebih senang membantu anda.
| Gred plat kapal tekanan yang dibekalkan oleh GNEE | |||||
| ASTM | ASTM A202/A202M | ASTM A202 Gred A | ASTM A202 Gred B | ||
| ASTM A203/A203M | ASTM A203 Gred A | ASTM A203 Gred B | ASTM A203 Gred D | ASTM A203 Gred E | |
| ASTM A203 Gred F | |||||
| ASTM A204/A204M | ASTM A204 Gred A | ASTM A204 Gred B | ASTM A204 Gred C | ||
| ASTM A285/A285M | ASTM A285 Gred A | ASTM A285 Gred B | ASTM A285 Gred C | ||
| ASTM A299/A299M | ASTM A299 Gred A | ASTM A299 Gred B | |||
| ASTM A302/A302M | ASTM A302 Gred A | ASTM A302 Gred B | ASTM A302 Gred C | ASTM A302 Gred D | |
| ASTM A387/A387M | ASTM A387 Gred 5 Class1 | ASTM A387 Gred 5 Class2 | ASTM A387 Gred 11 Class1 | ASTM A387 Gred 11 Class2 | |
| ASTM A387 Gred 12 Class1 | ASTM A387 Gred 12 Class2 | ASTM A387 Gred 22 Kelas1 | ASTM A387 gred 22 kelas2 | ||
| ASTM A515/A515M | ASTM A515 Gred 60 | ASTM A515 Gred 65 | ASTM A515 Gred 70 | ||
| ASTM A516/A516M | ASTM A516 Gred 55 | ASTM A516 Gred 60 | ASTM A516 Gred 65 | ASTM A516 Gred 70 | |
| ASTM A517/A517M | ASTM A517 Gred A | ASTM A517 Gred B | ASTM A517 Gred E | ASTM A517 Gred F | |
| ASTM A517 Gred P | ASTM A517 Gred J | ||||
| ASTM A533/A533M | ASTM A533 Gred A Class1 | ASTM A533 Gred B Class1 | ASTM A533 Gred C Class1 | ASTM A533 Gred D Class1 | |
| ASTM A533 Gred A Class2 | ASTM A533 Gred B Class2 | ASTM A533 Gred C Class2 | ASTM A533 Gred D Class2 | ||
| ASTM A533 Gred A Class3 | ASTM A533 Gred B Class3 | ASTM A533 Gred C Class3 | ASTM A533 Gred D Class3 | ||
| ASTM A537/A537M | ASTM A537 CLASS1 | ASTM A537 CLASS2 | ASTM A537 CLASS3 | ||
| ASTM A612/A612M | ASTM A612 | ||||
| ASTM A662/A662M | ASTM A662 Gred A | ASTM A662 Gred B | ASTM A662 Gred C | ||
| En | EN10028-2 | EN10028-2 P235GH | EN10028-2 P265GH | EN10028-2 P295GH | EN10028-2 P355GH |
| En 10028-2 16 mo3 | |||||
| EN10028-3 | EN10028-3 P275N | EN10028-3 P275NH | EN10028-3 P275NL1 | EN10028-3 P275NL2 | |
| EN10028-3 P355N | EN10028-3 P355NH | EN10028-3 P355NL1 | EN10028-3 P355NL2 | ||
| EN10028-3 P460N | EN10028-3 P460NH | EN10028-3 P460NL1 | EN10028-3 P460NL2 | ||
| EN10028-5 | EN10028-5 P355M | EN10028-5 P355ML1 | EN10028-5 P355ML2 | EN10028-5 P420M | |
| EN10028-5 P420ML1 | EN10028-5 P420ML2 | EN10028-5 P460M | EN10028-5 P460ML1 | ||
| EN10028-5 P460ML2 | |||||
| EN10028-6 | EN10028-6 P355Q | EN10028-6 P460Q | EN10028-6 P500Q | EN10028-6 P690Q | |
| EN10028-6 P355QH | EN10028-6 P460QH | EN10028-6 P500QH | EN10028-6 P690QH | ||
| EN10028-6 P355QL1 | EN10028-6 P460QL1 | EN10028-6 P500QL1 | EN10028-6 P690QL1 | ||
| EN10028-6 P355QL2 | EN10028-6 P460QL2 | EN10028-6 P500QL2 | EN10028-6 P690QL2 | ||
| Jis | JIS G3115 | JIS G3115 SPV235 | JIS G3115 SPV315 | JIS G3115 SPV355 | JIS G3115 SPV410 |
| JIS G3115 SPV450 | JIS G3115 SPV490 | ||||
| JIS G3103 | JIS G3103 SB410 | JIS G3103 SB450 | JIS G3103 SB480 | JIS G3103 SB450M | |
| JIS G3103 SB480M | |||||
| GB | GB713 | GB713 Q245R | GB713 Q345R | GB713 Q370R | Gb 713 12 cr1movr |
| Gb 713 12 cr2mo1r | Gb 713 13 mnnimor | GB 713 14 cr1mor | GB 713 15 crmor | ||
| Gb 713 18 mnmonbr | |||||
| GB3531 | Gb 3531 09 mnnidr | Gb 3531 15 mnnidr | Gb 3531 16 mndr | ||
| DIN | DIN 17155 | DIN 17155 HI | DIN 17155 HII | DIN 17155 10 crmo910 | Din 17155 13 crmo44 |
| DIN 17155 15 mo3 | Din 17155 17 mn4 | DIN 17155 19 mn6 | |||