P420ML1 dan P420ML2kedua -dua plat keluli termomechanically dilancarkan untuk kapal dan dandang tekanan, mengikut standard EN 10028 - 5. Perbezaan utama ialah ketahanan impak suhu rendah mereka: P420ml1 ditentukan untuk ujian impak AT-40 darjah, manakala P420ML2 ditentukan untuk ujian impak AT-50 darjah. Kedua -dua gred mempunyai kekuatan hasil minimum 420 MPa dan kebolehkalasan yang baik.
EN10028-5 Spesifikasi standard untuk keluli bijirin halus yang boleh dikimpal, Thermomechanically Rolled.
EN10028-5 merangkumi gred keluli yang diberikan dalam tiga kualiti:
a) siri asas (p ... m)
b) siri dengan sifat suhu rendah ke -40 darjah (P ... ML1);
c) Siri dengan sifat suhu rendah hingga ke -50 darjah (P ... ML2).
Teknologi Tambahan: Ujian HIC|NACE MR0175|Z15|Z25|Z35
Ketebalan: 6mm hingga 300mm,
Lebar: 1500mm hingga 4050mm,
Panjang: 3000mm hingga 15000mm
Harta mechnical untuk plat keluli P420ML1
| Ketebalan (mm) | Kekuatan hasil (lebih besar daripada atau sama dengan MPA) | Kekuatan tegangan (MPA) | Pemanjangan lebih besar daripada atau sama dengan,% |
| T kurang daripada atau sama dengan 16 | 420 | 500-660 | 19 |
| 16<> | 400 | ||
| 40<> | 390 |
Komposisi kimia untuk plat keluli p420ml1 (analisis haba maks%)
| Komposisi Elemen Kimia Utama Plat Keluli P420ml1 | ||||||
| C | SI | Mn | P | S | AL (Jumlah) | N |
| 0.16 | 0.50 | 1.70 | 0.020 | 0.015 | Lebih besar daripada atau sama dengan 0.020 | 0.020 |
| Mo | Nb | Ni | Ti | V | Cr+Cu+mo | |
| 0.20 | 0.05 | 0.50 | 0.05 | 0.10 | 0.60 | |
Harta mechnical untuk plat keluli P420ml2:
| Ketebalan (mm) | Kekuatan hasil (lebih besar daripada atau sama dengan MPA) | Kekuatan tegangan (MPA) | Pemanjangan lebih besar daripada atau sama dengan,% |
| T kurang daripada atau sama dengan 16 | 420 | 500-660 | 19 |
| 16<> | 400 | ||
| 40<> | 390 |
Komposisi kimia untuk plat keluli P420ml2 (analisis haba maks%)
| Komposisi Elemen Kimia Utama Plat Keluli P420ml2 | ||||||
| C | SI | Mn | P | S | AL (Jumlah) | N |
| 0.16 | 0.50 | 1.70 | 0.020 | 0.015 | Lebih besar daripada atau sama dengan 0.020 | 0.020 |
| Mo | Nb | Ni | Ti | V | Cr+Cu+mo | |
| 0.20 | 0.05 | 0.50 | 0.05 | 0.10 | 0.60 | |
Keperluan teknikal & perkhidmatan tambahan untuk plat keluli P420ML1/ML2
♦ Ujian ketegangan yang tinggi
♦ Ujian kesan suhu rendah
♦ Simulasi pos - rawatan haba yang dikimpal (PWHT)
♦ Ujian ultrasonik di bawah EN 10160, ASTM A435, A577, A578
♦ Sijil ujian kilang orginal di bawah format EN 10204 3.1/3.2
♦ Shot letupan dan lukisan, memotong dan mengimpal mengikut permintaan pengguna akhir
Sekiranya anda ingin mengetahui lebih lanjut mengenai produk GNEE, anda boleh menghantar e -mel kealloy@gneesteelgroup.com. Kami lebih senang membantu anda.
| Gred plat kapal tekanan yang dibekalkan oleh GNEE | |||||
| ASTM | ASTM A202/A202M | ASTM A202 Gred A | ASTM A202 Gred B | ||
| ASTM A203/A203M | ASTM A203 Gred A | ASTM A203 Gred B | ASTM A203 Gred D | ASTM A203 Gred E | |
| ASTM A203 Gred F | |||||
| ASTM A204/A204M | ASTM A204 Gred A | ASTM A204 Gred B | ASTM A204 Gred C | ||
| ASTM A285/A285M | ASTM A285 Gred A | ASTM A285 Gred B | ASTM A285 Gred C | ||
| ASTM A299/A299M | ASTM A299 Gred A | ASTM A299 Gred B | |||
| ASTM A302/A302M | ASTM A302 Gred A | ASTM A302 Gred B | ASTM A302 Gred C | ASTM A302 Gred D | |
| ASTM A387/A387M | ASTM A387 Gred 5 Class1 | ASTM A387 Gred 5 Class2 | ASTM A387 Gred 11 Class1 | ASTM A387 Gred 11 Class2 | |
| ASTM A387 Gred 12 Class1 | ASTM A387 Gred 12 Class2 | ASTM A387 Gred 22 Kelas1 | ASTM A387 gred 22 kelas2 | ||
| ASTM A515/A515M | ASTM A515 Gred 60 | ASTM A515 Gred 65 | ASTM A515 Gred 70 | ||
| ASTM A516/A516M | ASTM A516 Gred 55 | ASTM A516 Gred 60 | ASTM A516 Gred 65 | ASTM A516 Gred 70 | |
| ASTM A517/A517M | ASTM A517 Gred A | ASTM A517 Gred B | ASTM A517 Gred E | ASTM A517 Gred F | |
| ASTM A517 Gred P | ASTM A517 Gred J | ||||
| ASTM A533/A533M | ASTM A533 Gred A Class1 | ASTM A533 Gred B Class1 | ASTM A533 Gred C Class1 | ASTM A533 Gred D Class1 | |
| ASTM A533 Gred A Class2 | ASTM A533 Gred B Class2 | ASTM A533 Gred C Class2 | ASTM A533 Gred D Class2 | ||
| ASTM A533 Gred A Class3 | ASTM A533 Gred B Class3 | ASTM A533 Gred C Class3 | ASTM A533 Gred D Class3 | ||
| ASTM A537/A537M | ASTM A537 CLASS1 | ASTM A537 CLASS2 | ASTM A537 CLASS3 | ||
| ASTM A612/A612M | ASTM A612 | ||||
| ASTM A662/A662M | ASTM A662 Gred A | ASTM A662 Gred B | ASTM A662 Gred C | ||
| En | EN10028-2 | EN10028-2 P235GH | EN10028-2 P265GH | EN10028-2 P295GH | EN10028-2 P355GH |
| En 10028-2 16 mo3 | |||||
| EN10028-3 | EN10028-3 P275N | EN10028-3 P275NH | EN10028-3 P275NL1 | EN10028-3 P275NL2 | |
| EN10028-3 P355N | EN10028-3 P355NH | EN10028-3 P355NL1 | EN10028-3 P355NL2 | ||
| EN10028-3 P460N | EN10028-3 P460NH | EN10028-3 P460NL1 | EN10028-3 P460NL2 | ||
| EN10028-5 | EN10028-5 P355M | EN10028-5 P355ML1 | EN10028-5 P355ML2 | EN10028-5 P420M | |
| EN10028-5 P420ML1 | EN10028-5 P420ML2 | EN10028-5 P460M | EN10028-5 P460ML1 | ||
| EN10028-5 P460ML2 | |||||
| EN10028-6 | EN10028-6 P355Q | EN10028-6 P460Q | EN10028-6 P500Q | EN10028-6 P690Q | |
| EN10028-6 P355QH | EN10028-6 P460QH | EN10028-6 P500QH | EN10028-6 P690QH | ||
| EN10028-6 P355QL1 | EN10028-6 P460QL1 | EN10028-6 P500QL1 | EN10028-6 P690QL1 | ||
| EN10028-6 P355QL2 | EN10028-6 P460QL2 | EN10028-6 P500QL2 | EN10028-6 P690QL2 | ||
| Jis | JIS G3115 | JIS G3115 SPV235 | JIS G3115 SPV315 | JIS G3115 SPV355 | JIS G3115 SPV410 |
| JIS G3115 SPV450 | JIS G3115 SPV490 | ||||
| JIS G3103 | JIS G3103 SB410 | JIS G3103 SB450 | JIS G3103 SB480 | JIS G3103 SB450M | |
| JIS G3103 SB480M | |||||
| GB | GB713 | GB713 Q245R | GB713 Q345R | GB713 Q370R | Gb 713 12 cr1movr |
| Gb 713 12 cr2mo1r | Gb 713 13 mnnimor | GB 713 14 cr1mor | GB 713 15 crmor | ||
| Gb 713 18 mnmonbr | |||||
| GB3531 | Gb 3531 09 mnnidr | Gb 3531 15 mnnidr | Gb 3531 16 mndr | ||
| DIN | DIN 17155 | DIN 17155 HI | DIN 17155 HII | DIN 17155 10 crmo910 | Din 17155 13 crmo44 |
| DIN 17155 15 mo3 | Din 17155 17 mn4 | DIN 17155 19 mn6 | |||