What is P500Q steel plate?

Nov 27, 2025 Tinggalkan pesanan

Steel Standard:EN 10028-6

Thickness:6mm-300mm

Width:1500mm-4200mm

Length:3000mm-18000mm

 

Technical Requirements & Additional Services for P500Q steel plate:


Simulated post-welded heat treatment (PWHT)
Ultrasonic test under EN 10160,ASTM A435,A577,A578
Issued Orginal Mill test certificate under EN 10204 FORMAT 3.1/3.2

 

Mechnical property for P500Q steel plate:
 

P500Q≤ 50> 50 ≤ 100> 100
500480440
 ≤ 100> 100
590-770540-720


Chemical composition for P500Q steel plate (Heat Analysis Max%)

 

 

Main chemical elements composition of P500Q steel plate
CPSBN
0.180.601.700.0250.0150.0050.0151.00
V
0.300.700.051.500.050.080.15