Produk keluli struktur (IPE, UPE, UPN, HEA, HEB, sudut sama dan tidak sama) dalam gred S235JR, S275JR, S355J2

Mar 05, 2025 Tinggalkan pesanan

Bahan Dimensi (mm) Panjang (mm) Gred
L 25 x 25 x 4 12000 S235JR/S275JR
L 30 x 30 x 3 12000 S355
L 30 x 30 x 4 12000 S235JR/S275JR
L 30 x 30 x 4 12000 S355
L 35 x 35 x 4 12000 S355
L 35 x 35 x 5 12000 S355
L 40 x 40 x 4 12000 S235JR/S275JR
L 40 x 40 x 4 12000 S355
L 40 x 40 x 5 12000 S235JR/S275JR
L 40 x 40 x 5 12000 S355
L 50 x 50 x 5 12000 S355
L 50 x 50 x 6 12000 S235JR/S275JR
L 50 x 50 x 6 12000 S355
L 60 x 60 x 10 12000 S355
L 60 x 60 x 5 12000 S355
L 60 x 60 x 6 12000 S355
L 60 x 60 x 8 12000 S235JR/S275JR
L 60 x 60 x 8 12000 S355
L 65 x 65 x 5 12000 S355
L 65 x 65 x 6 12000 S355
L 65 x 65 x 7 12000 S355
L 65 x 65 x 8 12000 S355
L 70 x 70 x 10 12000 S355
L 70 x 70 x 6 12000 S355
L 70 x 70 x 7 12000 S355
L 70 x 70 x 8 12000 S235JR/S275JR
L 70 x 70 x 9 12000 S235JR/S275JR
L 75 x 50 x 5 12000 S355
L 75 x 50 x 6 12000 S355
L 75 x 50 x 7 12000 S235JR/S275JR
L 75 x 50 x 7 12000 S355
L 75 x 50 x 8 12000 S355
L 75 x 50 x 9 12000 S355
L 75 x 75 x 10 12000 S355
L 75 x 75 x 6 12000 S235JR/S275JR
L 75 x 75 x 6 12000 S355
L 75 x 75 x 7 12000 S355
L 75 x 75 x 8 12000 S355
L 80 x 40 x 6 12000 S355
L 80 x 80 x 10 12000 S235JR/S275JR
L 80 x 80 x 10 12000 S355
L 80 x 80 x 6 12000 S355
L 80 x 80 x 8 12000 S355
L 90 x 60 x 6 12000 S355
L 90 x 60 x 8 12000 S235JR/S275JR
L 90 x 90 x 10 12000 S355
L 90 x 90 x 11 12000 S355
L 90 x 90 x 12 12000 S355
L 90 x 90 x 13 12000 S355
L 90 x 90 x 8 12000 S355
L 90 x 90 x 9 12000 S355
L 100 x 100 x 10 12000 S355
L 100 x 100 x 11 12000 S355
L 100 x 100 x 12 12000 S355
L 100 x 100 x 16 12000 S355
L 100 x 100 x 8 12000 S355
L 100 x 50 x 10 12000 S235JR/S275JR
L 100 x 50 x 10 12000 S355
L 100 x 50 x 6 12000 S235JR/S275JR
L 100 x 50 x 6 12000 S355
L 100 x 50 x 8 12000 S355
L 100 x 65 x 10 12000 S355
L 100 x 65 x 7 12000 S355
L 100 x 65 x 8 12000 S355
L 100 x 65 x 9 12000 S355
L 100 x 75 x 10 12000 S355
L 100 x 75 x 11 12000 S355
L 100 x 75 x 12 12000 S355
L 100 x 75 x 7 12000 S235JR/S275JR
L 100 x 75 x 7 12000 S355
L 100 x 75 x 8 12000 S355
L 100 x 75 x 9 12000 S355
L 110 x 110 x 10 12000 S355
L 110 x 110 x 12 12000 S355
L 120 x 120 x 10 12000 S355
L 120 x 120 x 12 12000 S235JR/S275JR
L 120 x 120 x 12 12000 S355
L 120 x 120 x 15 12000 S235JR/S275JR
L 120 x 120 x 15 12000 S355
L 120 x 120 x 8 12000 S355
L 120 x 80 x 10 12000 S355
L 120 x 80 x 12 12000 S355
L 120 x 80 x 8 12000 S235JR/S275JR
L 120 x 80 x 8 12000 S355
L 125 x 75 x 10 12000 S355
L 125 x 75 x 12 12000 S355
L 125 x 75 x 8 12000 S355
L 130 x 130 x 10 12000 S355
L 130 x 130 x 12 12000 S355
L 130 x 130 x 14 12000 S235JR/S275JR
L 140 x 140 x 13 12000 S355
L 150 x 100 x 10 12000 S355
L 150 x 100 x 12 12000 S355
L 150 x 100 x 14 12000 S355
L 150 x 100 x 15 12000 S355
L 150 x 150 x 10 12000 S235JR/S275JR
L 150 x 150 x 10 12000 S355
L 150 x 150 x 14 12000 S235JR/S275JR
L 150 x 150 x 14 12000 S355
L 150 x 150 x 15 12000 S355
L 150 x 150 x 16 12000 S235JR/S275JR
L 150 x 150 x 16 12000 S355
L 150 x 150 x 18 12000 S355
L 150 x 150 x 20 12000 S235JR/S275JR
L 150 x 150 x 20 12000 S355
L 150 x 75 x 10 12000 S355
L 150 x 75 x 11 12000 S355
L 150 x 75 x 12 12000 S355
L 150 x 75 x 15 12000 S235JR/S275JR
L 150 x 75 x 15 12000 S355
L 150 x 75 x 9 12000 S355
L 150 x 90 x 10 12000 S355
L 150 x 90 x 12 12000 S355
L 150 x 90 x 15 12000 S235JR/S275JR
L 150 x 90 x 15 12000 S355
L 160 x 160 x 15 12000 S235JR/S275JR
L 160 x 160 x 15 12000 S355
L 160 x 160 x 17 12000 S235JR/S275JR
L 160 x 160 x 17 12000 S355
L 160 x 80 x 10 12000 S235JR/S275JR
L 180 x 180 x 16 12000 S235JR/S275JR
L 180 x 180 x 16 12000 S355
L 180 x 180 x 18 12000 S235JR/S275JR
L 180 x 180 x 18 12000 S355
L 180 x 180 x 20 12000 S235JR/S275JR
L 180 x 180 x 20 12000 S355
L 180 x 180 x 22 12000 S355
L 180 x 90 x 10 12000 S355
L 200 x 100 x 10 12000 S235JR/S275JR
L 200 x 100 x 10 12000 S355
L 200 x 100 x 12 12000 S235JR/S275JR
L 200 x 100 x 12 12000 S355
L 200 x 100 x 14 12000 S235JR/S275JR
L 200 x 100 x 14 12000 S355
L 200 x 100 x 15 12000 S235JR/S275JR
L 200 x 100 x 15 12000 S355
L 200 x 100 x 16 12000 S235JR/S275JR
L 200 x 100 x 16 12000 S355
L 200 x 150 x 12 12000 S235JR/S275JR
L 200 x 150 x 12 12000 S355
L 200 x 150 x 15 12000 S235JR/S275JR
L 200 x 150 x 15 12000 S355
L 200 x 200 x 16 12000 S235JR/S275JR
L 200 x 200 x 16 12000 S355
L 200 x 200 x 18 12000 S235JR/S275JR
L 200 x 200 x 18 12000 S355
L 200 x 200 x 20 12000 S235JR/S275JR
L 200 x 200 x 20 12000 S355
L 200 x 200 x 22 12000 S235JR/S275JR
L 200 x 200 x 22 12000 S355
L 200 x 200 x 24 12000 S235JR/S275JR
L 200 x 200 x 24 12000 S355
L 200 x 200 x 26 12000 S235JR/S275JR
L 200 x 200 x 26 12000 S355
L 200 x 200 x 28 12000 S235JR/S275JR
L 200 x 200 x 28 12000 S355
L 200 x 200 x 34 12000 S355
L 250 x 250 x 18 12000 S235JR/S275JR
L 250 x 250 x 18 12000 S355
L 250 x 250 x 20 12000 S235JR/S275JR
L 250 x 250 x 20 12000 S355
L 250 x 250 x 22 12000 S235JR/S275JR
L 250 x 250 x 22 12000 S355
L 250 x 250 x 24 12000 S235JR/S275JR
L 250 x 250 x 24 12000 S355
L 250 x 250 x 25 12000 S355
L 250 x 250 x 26 12000 S235JR/S275JR
L 250 x 250 x 26 12000 S355
L 250 x 250 x 28 12000 S355
L 250 x 250 x 30 12000 S355
L 250 x 250 x 35 12000 S355
L 250 x 90 x 10 12000 S235JR/S275JR
L 250 x 90 x 10 12000 S355
L 250 x 90 x 12 12000 S235JR/S275JR
L 250 x 90 x 12 12000 S355
L 250 x 90 x 14 12000 S235JR/S275JR
L 250 x 90 x 14 12000 S355
L 250 x 90 x 16 12000 S235JR/S275JR
L 250 x 90 x 16 12000 S355
Pr Hea 100 12000 S235JR/S275JR
Pr Hea 100 12000 S355
Pr HEA 120 12000 S235JR/S275JR
Pr HEA 120 12000 S355
Pr HEA 140 12000 S235JR/S275JR
Pr HEA 140 12000 S355
Pr HEA 160 12000 S235JR/S275JR
Pr HEA 160 12000 S355
Pr HEA 180 12000 S235JR/S275JR
Pr HEA 180 12000 S355
Pr HEA 200 12000 S235JR/S275JR
Pr HEA 200 12000 S355
Pr HEA 220 12000 S355
Pr HEA 260 12000 S355
Pr HEA 300 12000 S355
Pr Ibr 100 12000 S235JR/S275JR
Pr Ibr 100 12000 S355
Pr Heb 120 12000 S235JR/S275JR
Pr Heb 120 12000 S355
Pr Ibr 140 12000 S235JR/S275JR
Pr Ibr 140 12000 S355
Pr Ibr 160 12000 S235JR/S275JR
Pr Ibr 160 12000 S355
Pr Ibr 180 12000 S235JR/S275JR
Pr Ibr 200 12000 S235JR/S275JR
Pr Ibr 200 12000 S355
Pr Ipe 100 12000 S235JR/S275JR
Pr IPE 120 12000 S235JR/S275JR
Pr IPE 140 12000 S235JR/S275JR
Pr IPE 160 12000 S235JR/S275JR
Pr IPE 160 12000 S235JR/S275JR
Pr IPE 220 12000 S355
Pr IPE 240 12000 S355
Pr IPE 270 12000 S355
Pr IPE 300 12000 S355
Pr IPE 550 12000 S355
Pr IPE 80 12000 S235JR/S275JR
Pr IPN 360 12000 S235JR/S275JR
Pr IPN 80 12000 S235JR/S275JR
Pr UPE 80 12000 S355
Pr UPE 100 12000 S355
Pr UPE 120 12000 S355
Pr UPE 140 12000 S355
Pr UPE 160 12000 S355
Pr UPE 180 12000 S355
Pr UPE 200 12000 S235JR/S275JR
Pr UPE 200 12000 S355
Pr UPE 220 12000 S355
Pr UPE 240 12000 S355
Pr UPE 300 12000 S355
Pr UPE 400 12000 S355

Kami mempunyai ruang penyimpanan lebih daripada 10000 m² dan mengekalkan hubungan rapat dengan beratus -ratus pembekal dan kilang keluli di seluruh Eropah dan di seluruh dunia. Ini membolehkan kami dengan cepat menyampaikan saiz atau gred yang tidak tersedia dalam stok kami pada harga terbaik dan masa memimpin.

Stok kami terutamanya termasuk:

• Produk keluli struktur (IPE, UPE, UPN, HEA, HEB, sudut sama dan tidak sama) dalam gred S235JR, S275JR, S355J2

• Lembaran dan gegelung keluli panas (3mm hingga 12mm, DD11/S235JR+N/S355MC, jeruk dan minyak)

• Lembaran dan gegelung keluli tergalvani (0. 5mm hingga 4mm, dx 51+ z)

• Lembaran dan gegelung keluli yang dilancarkan sejuk (DC01)

• T-bar, bar rata, bar bulat, bar persegi, dan bahagian berongga (EN 10219 atau EN 10210)

• Produk keluli tahan karat (bar, lembaran, pinggan)

• Plat berat (6mm hingga 300mm dalam saiz dan gred)