A203 Grade B Nickel Alloy Steel Plates

A203 Grade B Nickel Alloy Steel Plates

A203 Grade B Nickel Alloy Steel Plates is an ASTM standard nickel alloy steel plate used for low-temperature welded pressure vessels and boilers, featuring 2.25% nickel for excellent low-temp toughness, requiring normalization, and offering specific mechanical properties with minimum yield strength around 275 MPa, critical in oil, gas, and chemical projects for severe service.
Hantar pertanyaan
Berbual sekarang
Description/kawalan
Parameter teknikal

Gneesteel is specialized in supplying ASTM A203 steel plate in A203 Grade B. For more information of A203 Grade B steel plates, please check them in following:

 

A203 Grade B Nickel Alloy Steel Plates Chemical Composition

C

P

S

A203 Grade B

0.17

0.13-0.45

0.78-0.88

0.035

0.035

Carbon Equivalent: Ceq=【C+Mn/6+(Cr+Mo+V)/5+(Ni+Cu)/15】%

 

A203 Grade B mechanical properties


ASTM A 203

2 in. (50 mm) & under

70-90

[485-620]

over 2 in. (50 mm)

70-90

[485-620]

Yield strength, min.

2 in. (50 mm) & under

40

[275]

over 2 in. (50 mm)

40

[275]

Elongation in 8 in. (200 mm), min, %

17

Elongation in 2 in. (50 mm), min, %

21

 

The inspection and testing required for ASTM A203 nickel-alloy steel plates include: chemical analysis, tension test, Charpy V-Notch impact test, drop weight test, high-temperature tension test, ultrasonic examination, as well as magnetic particle examination.

A203 Grade B Nickel Alloy Steel

A203 Grade B Nickel Alloy Steel Plate

If you have some question or demands,please contact us at free time.

Cool tags: a203 grade b nickel alloy steel plates, China a203 grade b nickel alloy steel plates manufacturers, suppliers, factory, A516GR55 A516GR60 PLAT, ASTM A516 Tekanan Kapal Karbon Keluli, Plat Kapal Tekanan ASTM A516 GR 70, gred keluli tekanan tekanan, Plat dandang keluli SA516, keluli plat dandang kimpalan