EN10028-2 P265GH Pressure Steel Plate

EN10028-2 P265GH Pressure Steel Plate

P265GH is a type of weldable, non-alloy steel designed for use in pressure vessels and boilers, especially for elevated temperature service. It is characterized by a minimum yield strength of 265 MPa (for thicknesses up to 16 mm) and a tensile strength between 410 and 570 MPa. Its good weldability and properties at high and low temperatures make it a common choice for the oil & gas, petrochemical, and chemical industries.
Hantar pertanyaan
Berbual sekarang
Description/kawalan
Parameter teknikal

P265GH is a carbon structural steel for boilers and pressure vessels under the European standard (EN standard). It belongs to the EN 10028-2 standard system and is primarily used for manufacturing structural components for medium-temperature pressure conditions. It is widely used in petrochemical, power, and shipbuilding industries.


Mechanical properties of steel P265GH (1.0425)

to 100 100 - 150 150 - 250
Rm - Tensile strength (MPa) (+N) 410-530 400-530 390-530

 

to 16 16 - 40 40 - 60 60 - 100 100 - 150 150 - 250
ReH - Minimum yield strength (MPa) (+N) 265 255 245 215 200 185

 

KV - Impact energy (J) transverse, (+N) -20℃
27
0℃
27
+20℃
40
KV - Impact energy (J) longitud., -10℃
28
0℃
40
+20℃
47

 

A - Min. elongation at fracture (%) (+N) 22-23
A - Min. elongation at fracture (%) transverse, (+N) 21

EN10028-2 P265GH Pressure Steel Plate

EN10028-2 P265GH Pressure Steel Plate

GNEE have served clients in over 50 countries (North America, Europe, Southeast Asia, the Middle East, etc.) and gained rich experience in international trade terms (FOB, CIF, EXW) and local market requirements. Our efficient communication (English, Spanish, Arabic support) and transparent business processes make cooperation smooth and hassle-free.

Cool tags: en10028-2 p265gh pressure steel plate, China en10028-2 p265gh pressure steel plate manufacturers, suppliers, factory, 16mo3 Plat Ssteel Hot Rolled Hot, Plat berkualiti dandang, Dandang keluli perindustrian, Plat keluli tekanan P275NH, Keluli kapal tekanan p420ml2, SA516 70 Plate