P355M Pressure Vessel Steel is an alloy steel formulated for primary forming into wrought products. Cited properties are appropriate for the thermomechanically rolled condition. P355M Pressure Vessel Steel is the EN numeric designation for this material.
P355M Pressure Vessel Steel is the EN chemical designation.
It has a moderately high thermal conductivity and a very low tensile strength among EN wrought alloy steels.
Chemical composition % of steel P355M Pressure Vessel Steel (1.8821): EN 10028-5-2003
| Main chemical elements composition of P355M steel plate | ||||||
| C | P | S | N | |||
| 0.14 | 0.50 | 1.60 | 0.025 | 0.020 | >=0.020 | 0.015 |
| V | Cr+Cu+Mo | |||||
| 0.20 | 0.05 | 0.50 | 0.05 | 0.10 | 0.60 | |
Mechnical property for P355M steel plate:
| T<=16 | 355 | 450-610 | 22 |
| 16<> | 355 | ||
| 40<> | 345 |


A:We accept FOB,CIF,CFR and other international shipping terms.Port of loading can be specified according to customer requirements.
Q:Do you have after-sales service?
A:Of course, you can contact us at any time.we promise our products are all qualified. If you find any products are not qualified and unsatisfied your require,please contact us at any time.
Cool tags: p355m pressure vessel steel, China p355m pressure vessel steel manufacturers, suppliers, factory, Dandang keluli perindustrian, P235GH P265GH Plat Keluli Boiler, Plat keluli tekanan P275NH, P275NH Steel, P355NL1 P355NL2 Plat Keluli Boiler, Plat berkualiti dandang P460N P460NH