375" Dia x 36" Zirconium 702 Round Bar
702 zirconium round bar is fully resistant to alkaline solutions and molten alkalis. Its corrosion resistance in sodium hydroxide media is the same as that of nickel, and due to its excellent corrosion resistance, 702 zirconium round steel is in many cases much better than tantalum and precious metals. In addition, zirconium 702 steel round bar also has good mechanical properties and high temperature resistance, therefore, zirconium 702 steel rounds in chemical equipment, especially in the corrosion resistance requirements of high equipment zirconium 702 round stock steel is mainly used in the manufacture of chemical equipment in the heat exchanger, container lining, valves, pump shells, blades, stirrers, conduits, etc., many of the production of fertilizers, resins, plastics, acid chemical equipment are used Zirconium 702 round bar stock.
zircinium 702 round metal bar chemical composition
|
Zr702 |
Zr+Hf |
Fe+Cr |
N |
H |
C |
O |
||
|
>=99.2 |
<=4.5 |
- |
0.2 |
0.025 |
0.005 |
0.05 |
0.16 |
|
Main properties of zirconium 702 round rod
Corrosion resistance: Zirconium 702 round stock metal is extremely resistant to corrosive substances. This makes it the preferred choice for applications exposed to harsh chemicals.
Strength-to-weight ratio: Zirconium 702 solid round bar is strong and lightweight, which helps maintain structural integrity without adding excessive weight.
Heat resistance: Zirconium 702 round bar stock steel maintains its integrity at elevated temperatures, a valuable characteristic for applications in high heat environments.
Low neutron absorption: Zirconium 702 round steel rod has a low neutron absorption cross-section, which plays a key role in nuclear applications, facilitating effective neutron regulation.
Non-magnetic: The non-magnetic properties of zirconium 702 steel rod bar are beneficial in applications where electromagnetic interference needs to be minimized.
Environmental Stability: Zirconium 702's round metal stock resistance to oxidation and degradation ensures its longevity and makes it suitable for a wide range of environments.
zirconium 702 round metal rod product image




Our products have undergone strict quality testing and come with professional certificates. If you have any questions about 375" Dia x 36" Zirconium 702 Round Bar, please feel free to inspect.
Cool tags: 375" dia x 36" zirconium 702 round bar, China 375" dia x 36" zirconium 702 round bar manufacturers, suppliers, factory, အကြမ်းခံဂိုဏ်းဒိုနီယမ်သတ္တုစပ်, Zirconium သတ္တုစပ်၏လောင်စာဆဲလ်စက်, sensor zirconium သတ္တုစပ်, ဖွံ့ဖြိုးမှုဇာရေးဒွန်နီယမ်သတ္တုစပ်, zirconium သတ္တုစပ်၏ပြန်လည်အသုံးပြုနိုင်သည်, ဇာကွန်နီယမ်သတ္တုစပ်စိမ်းလန်းသောစက်