Gneesteel is a leading supplier of high-quality pressure vessel steel plates, specializing in ASTM A515 Gr 60 steel plates. Designed for intermediate and higher-temperature service, ASTM A515 Gr.60 is a carbon steel plate widely used in pressure vessel manufacturing due to its excellent ductility, weldability, and cost-effectiveness.
Carbon A515 Grade 60 Steel Plate
|
C |
P |
S |
|||||||
|
t<=25 |
25<> |
50<> |
100<> |
200<> |
|||||
|
A515 grade 60 |
0.24 |
0.27 |
0.29 |
0.31 |
0.31 |
0.90 max |
0.035 max |
0.035 max |
0.15~0.40 |
Carbon A515 Grade 60 Steel Plate
|
A515 grade 60 |
32 (220) min |
60~80 (415~550) |
8 in. [200 mm], min, % |
21 min |
|
2 in. [50 mm], min, % |
25 min |
|||
UT(Ultrasonic examination), AR(As Hot Rolled only), TMCP(Thermal Mechanical Control Processing), N(Normalized), Q+T(Quenched and Tempered),Z Direction Test(Z15,Z25,Z35), Charpy V-Notch Impact Test, The Third Party Test (such as SGS Test), Coated or Shot Blasting and Painting.
Packaging Details: Standard export seaworthy packing or as required.
Delivery Time: 30-50 days, 7 days for stock goods.
Loading Port: Shanghai ,Tianjin, Qingdao.
Offer Ability:5 000MT/Per Month.
MOQ: 1 Pcs.


Cool tags: carbon a515 grade 60 steel plate, China carbon a515 grade 60 steel plate manufacturers, suppliers, factory, Plat keluli A537, Plat keluli dandang, gred keluli tekanan tekanan, Plat berkualiti dandang SA455, Kapal tekanan tahan karat, keluli plat dandang kimpalan