Gneesteel is a leading supplier of high-quality pressure vessel steel plates, specializing in ASTM A515 Gr 60 steel plates. Designed for intermediate and higher-temperature service, ASTM A515 Gr.60 is a carbon steel plate widely used in pressure vessel manufacturing due to its excellent ductility, weldability, and cost-effectiveness. Gneesteel provides an in-depth look at the chemical composition, mechanical properties, and applications of ASTM A515GR.60.
|
0.24-0.31 |
0.24-0.31 |
|
|
0.98 |
0.90 |
|
|
0.035 |
0.035 |
|
|
0.035 |
0.035 |
|
|
0.13-0.45 |
0.15-0.40 |
Ceq=[C + Mn/6 + (Cr + Mo + V)/5 + (Ni + Cu)/15]%.
Carbon A515 Grade 60 Steel offers excellent ductility and moderate strength, making it a preferred choice for less demanding high-temperature applications. The following table outlines its key mechanical characteristics:
|
<= 200 |
220 |
415-550 |
21 |
|
<= 50 |
220 |
415-550 |
25 |
These properties ensure that ASTM A515GR.60 steel plates can withstand moderate pressure conditions while maintaining structural integrity.