Manganese Molybdenum Alloy A302 Grade A Steel

Manganese Molybdenum Alloy A302 Grade A Steel

A302 Grade A refers to a specific type of manganese-molybdenum (Mn-Mo) alloy steel plate (ASTM A302 Gr.A) used primarily for manufacturing welded boilers and pressure vessels, offering good strength for elevated temperatures in oil, gas, and related industries, with standardized chemical composition and mechanical properties.
Hantar pertanyaan
Berbual sekarang
Description/kawalan
Parameter teknikal

A302 Grade A is a manganese-molybdenum alloy steel plate material specified under the ASTM A302/A302M standard, primarily used for welded boilers and other pressure vessels.

 

Main chemical elements composition of A302Grade A steel plate
C P S
T<=25 0.20 0.13-0.45 0.87-1.41 0.035 0.035 0.41-0.64
25<> 0.23
50<> 0.25

 

Mechnical property for A302GrA steel plate:

310 515-655 200mm 50mm
15 19

 

Technical Requirements & Additional Services for A302 GRA steel plate:
1,High tension test

2, Low temperature impacting test
3, Normalised for thick plates over 40mm
4,Simulated post-welded heat treatment (PWHT)
5, Rolling under standard NACE MR-0175 (HIC+SSCC)
6,Issued Orginal Mill test certificate under EN 10204 FORMAT 3.1/3.2
7,Shot blasting and Painting,Cutting and welding as per end user's demands

 

Manganese Molybdenum Alloy A302 Grade A Steel

Manganese Molybdenum Alloy A302 Grade A Steel

 

Cool tags: manganese molybdenum alloy a302 grade a steel, China manganese molybdenum alloy a302 grade a steel manufacturers, suppliers, factory, A516GR55 A516GR60 PLAT, ASTM Asme ဖိအားရေယာဉ်သံမဏိသံမဏိ, plat ASTM A516 GR 70, Plat Kapal Tekanan, Plat Kapal Tekanan ASTM A516 GR 70, Plat dandang keluli SA516