ASTM A299 Grade A boiler steel plate,ASME SA299 Grade A pressure vessel steel plate are specification for carbon steel and Manganese-Silicon.As for thin plate SA299 Grade A which produced from steel coil SA299 Grade A and furnished without heat treatment or just with stress relieving only,the additional requirements,including additional testing requirements and the reporting of additional test results shall be applied for A20/A20M steel standard.
|
A299 Grade A |
Main chemical composition of A299 Grade A |
||||
|
C |
P |
S |
|||
|
T<=25 |
0.28 |
0.13-0.45 |
0.84-1.52 |
0.035 |
0.035 |
|
T>25 |
0.30 |
0.84-1.62 |
|||
|
Equivalent steel grade of A299 Grade A |
||||||||
|
U.K |
||||||||
|
|
|
T St E255 |
|
Fe 360 2 KG |
|
|
|
|


A:We accept FOB,CIF,CFR and other international shipping terms.Port of loading can be specified according to customer requirements.
Q:Do you have after-sales service?
A:Of course, you can contact us at any time.we promise our products are all qualified. If you find any products are not qualified and unsatisfied your require,please contact us at any time.
Cool tags: manganese silicon carbon a299 grade a, China manganese silicon carbon a299 grade a manufacturers, suppliers, factory, Plat Keluli Kapal Tekanan A515, A516GR55 A516GR60 PLAT, Plat keluli A537, ASTM A516 GR 70 Plate, ASTM Asme ဖိအားရေယာဉ်သံမဏိသံမဏိ, Plat berkualiti dandang SA455